Diamond wire cutting for jade, agate, obsidian and other lapidary materials — low kerf loss, controlled feed, and a cut that protects the stone rather than the schedule.

필터
애플리케이션 랩
소재를 보내주시면 무료 테스트 절단 보고서를 드립니다
소재, 두께, 목표 공차를 알려주세요. 자체 다이아몬드 와이어쏘로 시편을 절단하고 와이어 사양, 이송 속도, 표면 조도, 사이클 타임을 회신합니다.

Why lapidary work moved to wire

A slab saw with a diamond blade removes a kerf of 3–5 mm. On a piece of high-value rough, that kerf is the single largest material loss in the whole process. A 0.45 mm wire removes less than a tenth of that, which changes the economics of cutting valuable rough at all.

The second reason is control. Wire cuts with a constant, 저힘, so it does not propagate existing fractures the way a large blade does. On included material that is the difference between a slab and a pile of fragments.

Wire selection by material

재료Wire ØAbrasiveFeedRisk
네프라이트 / 옥비트0.30–0.50 mmD126–D1811–4 mm/minFracture propagation from existing flaws
석영 / chalcedony0.25–0.40 mmD64–D1261–3 mm/분Chatter on hard/soft banding
Obsidian / volcanic glass0.20–0.30 mmD30–D640.5–2 mm/minConchoidal fracture at exit
Turquoise / soft opaque0.20–0.30 mmD300.3–1 mm/minAbsorbs coolant; staining

Handling the rough is the real skill

Before the cut: inspect under raking light for fractures, and decide the orientation from the stone, not from the machine. A flaw running across the intended cut plane will open regardless of feed. Rotating the cut by 15° often avoids it entirely.

During the cut: keep the feed constant and let the wire do the work. Operators tend to push the last third of the cut; that is exactly where the stone is weakest because the wire is exiting.

Coolant and staining

Porous lapidary materials absorb fluid. Use a clean water-based coolant with no dye and no rust inhibitor that leaves residue, and rinse the slab immediately. A stain that appears a week later is a coolant problem, not a stone problem.

자주 묻는 질문

Can wire cut a stone with visible fractures?

Sometimes, if the fracture does not intersect the cut plane and you support both sides. More often the correct answer is to cut around it — the wire will follow the fracture rather than resist it.

Is wire slower than a slab saw?

Slower per cut, 네. But it loses a tenth of the material and does not shatter included rough, so on valuable stone the effective yield is higher.

What wire do I start with for unknown material?

0.35 밀리미터, D126, feed at the low end of the range. Then adjust feed first, grit second, diameter last — diameter changes have the biggest effect on kerf and the smallest on cut quality.